Etched, Not Punched
Etch marks below Sch 40S
Seams Declared
W suffix on welded parts
Pickled Bright
Clean oxide-free surface
No Iron Pickup
Kept off steel racks
Case-Level Heat Tags
Tag matches the MTC
Titanium fittings leave our Khetwadi works pickled, grade-marked and packed away from carbon steel contact.
Operating Since 2021
Manifest Alloys, Khetwadi
ISO 9001:2015
Audited quality routine
GST Registered
Tax-compliant invoicing
Udyam (MSME)
MSME ministry enrolment
Import-Export Code
IEC issued by DGFT
Forming & Bevel Bay
Cut, formed, bevelled in-house
Export Paper Pack
MTC, COO, packing list
Flexible Payments
Several settlement routes
Seawater, wet chlorine, and hot brine can wear down steel pipe spools long before they reach their expected life. Titanium handles these conditions much better. It forms a thin, tight oxide layer on its surface that protects it, so it holds up very well in seawater. For fittings, ASTM B363 is the material standard, while ASME B16.9 and MSS SP-43 cover dimensions and shape. Commercially pure titanium grades work well for most water services. When conditions are tougher, alloyed grades add palladium, nickel-molybdenum, or vanadium for extra strength or corrosion resistance.
Our Khetwadi desk cuts, forms, bevels and pickles every titanium fitting before packing. Welded pieces carry the W suffix. Each lot ships with its EN 10204 certificate. Among Titanium Fittings Manufacturers in india, we keep titanium off carbon-steel racks. Buyers use us as Titanium Pipe Fittings Suppliers for mixed elbows, tees and stub ends. Gulf, African and Canadian orders leave Nhava Sheva with documents cleared early.
Key details a piping engineer checks before placing the order.
Build Route
Dimensional Codes
Product Analysis
Marking Rules
Optional NDT
Stress Relief (S3)
Surface Finish
Stub End Patterns
Physical Data
Bore Range
Wall Schedules
Applicable Standards
Bend Angles
Bend Radius
Bending Methods
End Types
Welding Process
Material Origin
Product Forms
Tests Offered
Documents
Packing
Palladium or nickel-molybdenum grades suit hot brine, while standard CP grades cover most seawater duty.
As a Titanium Pipe Fittings Supplier in India, we serve plants where corrosion costs most.
Intake, brine and product lines
Cooling and fire mains
Wet chlorine headers
Oxidising acid duty
Seawater cooling returns
Bleach liquor piping
Shell and tube nozzles
Ballast and engine cooling lines
Corrosive process piping
Light, high-strength Ti lines
Reverse osmosis skids
Clean, inert process lines
Cooling water circuits
Acid leach circuits
Nozzles and piping tie-ins
Every pattern is formed, bevelled, pickled and heat-tagged.
















Pick radius and angle to suit space and flow.
| Radius | Common Name | Typical Use |
|---|---|---|
| 1D | Short radius | Tight skids and spools |
| 1.5D | Long radius | Standard plant piping |
| 3D | Gentle bend | Lower pressure drop |
| 5D | Large bend | Pigging and slurry lines |
| 6D to 10D | Sweep bend | Custom long runs |
Angles: 22.5°, 30°, 45°, 60°, 90° and 180°.
Three seawater materials compared on flow, weight, temperature and cost.
Warm, chlorinated or fast-flowing seawater usually tips the final choice toward CP titanium fittings.
Titanium Pipe Fittings Manufacturer In Mumbai - Forming Bay Running At Khetwadi Since 2021
Send your line list with sizes and grades; our desk returns a consolidated priced schedule.
Match your drawing grade to its B363 symbol, UNS and W.Nr.
Welded fittings add the letter W. A welded Gr 2 elbow reads WPT2W.
Heat limits in weight percent from ASTM B265.
| Element (%) | WPT1 | WPT2 | WPT3 | WPT5 | WPT7 | WPT9 | WPT12 |
|---|---|---|---|---|---|---|---|
| Nitrogen (N), max | 0.03 | 0.03 | 0.05 | 0.05 | 0.03 | 0.03 | 0.03 |
| Carbon (C), max | 0.08 | 0.08 | 0.08 | 0.08 | 0.08 | 0.08 | 0.08 |
| Hydrogen (H), max | 0.015 | 0.015 | 0.015 | 0.015 | 0.015 | 0.015 | 0.015 |
| Iron (Fe), max | 0.20 | 0.30 | 0.30 | 0.40 | 0.30 | 0.25 | 0.30 |
| Oxygen (O), max | 0.18 | 0.25 | 0.35 | 0.20 | 0.25 | 0.15 | 0.25 |
| Aluminium (Al) | – | – | – | 5.5–6.75 | – | 2.5–3.5 | – |
| Vanadium (V) | – | – | – | 3.5–4.5 | – | 2.0–3.0 | – |
| Palladium (Pd) | – | – | – | – | 0.12–0.25 | – | – |
| Molybdenum (Mo) | – | – | – | – | – | – | 0.2–0.4 |
| Nickel (Ni) | – | – | – | – | – | – | 0.6–0.9 |
| Residuals, each max | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 |
| Residuals, total max | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 |
| Titanium (Ti) | Balance | Balance | Balance | Balance | Balance | Balance | Balance |
Single values are maximums. Titanium is the balance.
Only the stub end touches fluid, so flanges can use cheaper metal.
A Ti stub end with steel flange costs far less than solid titanium.
Annealed minimums from ASTM B861 and B265 tensile tables.
| Grade | Tensile Strength, min MPa (ksi) | 0.2% Yield, min MPa (ksi) | 0.2% Yield, max MPa (ksi) | Elongation in 50 mm, min % |
|---|---|---|---|---|
| WPT1 | 240 (35) | 138 (20) | 310 (45) | 24 |
| WPT2 | 345 (50) | 275 (40) | 450 (65) | 20 |
| WPT3 | 450 (65) | 380 (55) | 550 (80) | 18 |
| WPT5 | 895 (130) | 828 (120) | – | 10 |
| WPT7 | 345 (50) | 275 (40) | 450 (65) | 20 |
| WPT9 (annealed) | 620 (90) | 483 (70) | – | 15 |
| WPT12 | 483 (70) | 345 (50) | – | 18 |
Unalloyed grades also carry a yield ceiling for cold forming.
Titanium Stub Ends Stockist For Pune and Ahmedabad Buyers - Mumbai Racks Filled Since 2021
Our Titanium Pipe Fittings Stockist in Mumbai holds common elbows, tees and stub ends ready.
Centre-to-end values in millimetres for piping isometrics.
| NPS | OD at Bevel (mm) | 90° LR, A (mm) | 90° SR, A (mm) | 45° LR, B (mm) |
|---|---|---|---|---|
| ½ | 21.3 | 38 | – | 16 |
| 1 | 33.4 | 38 | 25 | 22 |
| 1½ | 48.3 | 57 | 38 | 28 |
| 2 | 60.3 | 76 | 51 | 35 |
| 3 | 88.9 | 114 | 76 | 51 |
| 4 | 114.3 | 152 | 102 | 64 |
| 6 | 168.3 | 229 | 152 | 95 |
| 8 | 219.1 | 305 | 203 | 127 |
| 10 | 273.0 | 381 | 254 | 159 |
| 12 | 323.8 | 457 | 305 | 191 |
Long radius equals 1.5 times NPS from NPS ¾ upwards.
Short and long pattern values in millimetres.
| NPS | Short Length F | Long Length F | Lap Dia G | Radius R |
|---|---|---|---|---|
| ½ | 51 | 76 | 35 | 3 |
| ¾ | 51 | 76 | 43 | 3 |
| 1 | 51 | 102 | 51 | 3 |
| 1¼ | 51 | 102 | 64 | 5 |
| 1½ | 51 | 102 | 74 | 6 |
| 2 | 64 | 152 | 92 | 8 |
| 2½ | 64 | 152 | 105 | 8 |
| 3 | 64 | 152 | 127 | 10 |
| 4 | 76 | 152 | 157 | 11 |
| 6 | 89 | 203 | 216 | 13 |
| 8 | 102 | 203 | 270 | 13 |
| 10 | 127 | 254 | 324 | 13 |
| 12 | 152 | 254 | 381 | 13 |
Inspection scope is agreed in writing before production.
Chemical & Mechanical
Visual & Surface
Non-Destructive
Certificates
Oxide colour shows how well argon shielding worked.
Colour only screens a weld. Bend or hardness tests confirm doubts.
Titanium Buttweld Fittings Exporter In India Serving Jebel Ali, UAE Desalination Projects
Consolidated crates reach Jebel Ali with MTC, COO and packing list matched to each tag.
Titanium is noble in seawater, so partner metals suffer.
Which metal corrodes in a titanium-steel joint?
The steel side; titanium stays cathodic.
Is cupro-nickel safe beside titanium?
No, it sits anodic and corrodes first.
What stops galvanic attack?
Remove contact, conductor or electrolyte.
Does area ratio matter?
Yes; small anode, large cathode is worst.
Where do isolation kits go?
Flanged joints between dissimilar spools.
Can super duplex spools join titanium?
Both sit near the noble end; risk is low.
Surface, shop and dispatch notes for Ti fittings.
Surface Finish
Machining Notes
Export Packing
Grade, bore and schedule decide each fitting rate.
Seamless or welded route also changes the price.
As a Titanium Pipe Fittings Stockist in India, we also sell single pieces for repairs.
The clock starts once grade, sizes and inspection are confirmed.
Stocked stub ends, elbows and tees leave Khetwadi within the week.
Sails from Nhava Sheva; Gulf ports first, Canada last.
Shutdown spares fly from Mumbai airport.
Transit grows with distance from Mumbai.
Being a Titanium Pipe Fittings Supplier in Mumbai keeps our local dispatch fast and dependable.
As a Titanium Pipe Fittings Exporter, we attach these codes and papers to invoices.
Buyers abroad shortlist us as a Titanium Pipe Fittings supplier that ships certified, mixed-size crates.
Middle East & Turkey
Africa
Americas
Europe
Asia Pacific
India
ASTM B363 Fittings Supplier In Toronto With Heat-Traceable, Grade-Etched Pieces
Canadian fabricators receive stub ends and elbows whose etched heat numbers match the enclosed certificate.
ASTM B363 covers seamless and welded titanium fittings, while ASME B16.9 fixes their dimensions.
It marks welded construction, so a seam-welded standard CP elbow is stamped WPT2W, not WPT2.
Indian customs classes them under 8108 90 90, the tariff line for other titanium articles.
Titanium resists erosion-corrosion at high flow, whereas 90/10 cupro-nickel pipework is limited by velocity.
Avoid wet contact and fit isolation kits, since steel corrodes faster when coupled to titanium.
No, commercially pure titanium fittings are non-magnetic, so magnet checks cannot confirm their grade.
Short pattern stub ends follow MSS SP-43, whereas long pattern ones follow ASME B16.9 dimensions.
Grade, size, wall schedule, seamless or welded route and testing scope together set each quote.